Abstract

Inorganic solid-state battery electrolytes show high ionic conductivities and enable the fabrication of all solid-state batteries. In this work, we present the temperature dependence of spin-lattice relaxation time (T1), spin-spin relaxation time (T2), and resonance linewidth () of the 7Li nuclear magnetic resonance (NMR) for four solid-state battery electrolytes (Li3InCl6 (LIC), Li3YCl6 (LYC), Li1.48Al0.48Ge1.52(PO4)3 (LAGP) and LiPS5Cl (LPSC) from 173 K to 403 K at a 7Li resonance frequency of 233 MHz, and from 253 K to 353 K at a 7Li resonance frequency of 291 MHz. Additionally, we measured the spin-lattice relaxation rates at an effective 7Li resonance frequency of 133 kHz using a spin-locking pulse sequence in the temperature range of 253 K to 353 K. In LPSC, the 7Li NMR relaxation is consistent with the Bloembergen-Pound-Purcell (BPP) theory of NMR relaxation of dipolar nuclei. In LIC, LYC and LAGP, the BPP theory does not describe the NMR relaxation rates for the temperature range and frequencies of our measurements. The presented NMR relaxation data assists in providing a complete picture of Li diffusion in these four solid-state battery electrolytes.

Comments

Comments are not moderated before they are posted, but they can be removed by the site moderators if they are found to be in contravention of our Commenting Policy [opens in a new tab] - please read this policy before you post. Comments should be used for scholarly discussion of the content in question. You can find more information about how to use the commenting feature here [opens in a new tab] .
This site is protected by reCAPTCHA and the Google Privacy Policy [opens in a new tab] and Terms of Service [opens in a new tab] apply.