Dithioacetal Polymers Capable of Chemical Recycling to Macrocyclic Monomers and Formation of Vitrimers

19 September 2022, Version 1
This content is a preprint and has not undergone peer review at the time of posting.

Abstract

Polymers capable of chemical recycling to monomers are highly desirable to produce sustainable materials with a circular economy. We here report a highly efficient ring-chain recycling of linear polydithioacetal (PDTA) via ring-closing depolymerization (RCD) and entropy-driven ring-opening polymerization (ED-ROP). Furthermore, once crosslinked, the network behaves as a vitrimer enabled by temperature-activated interchain exchange of dithioacetals in the bulk state. The vitrimer depolymerizes into macrocyclic monomers in solvent which can repolymerize to regenerate the vitrimer. Pristine linear PDTAs can be conveniently synthesized via a one-step reaction using 3,4,5-trimethoxybenzaldehyde and α,ω-alkyl dithiols with an acid catalyst. The resulting PDTAs undergo acid-catalyzed RCD with refluxing toluene to yield a mixture of macrocycles of various sizes with conversions of 75-95%. ED-ROP of these macrocyclic monomer mixtures in solution at room temperature affords virgin PDTAs, reaching high conversions of 80-95% within 2 h. Owing to the stability of dithioacetals, PDTAs are far more stable than the acetal counterparts, resisting hydrolysis under both acidic and basic conditions. With a floor temperature below 0 °C, depolymerization is not a concern in the bulk state even in the presence of residual catalysts as polymerization is favored at higher temperatures for ED-ROP.

Keywords

polydithioacetal
chemical recycling to monomer
entropy-driven ring-opening polymerization
transthioacetalization
macrocycle

Supplementary materials

Title
Description
Actions
Title
Supplementary Information
Description
The supplementary information includes details of the syntheses of polymers, depolymerizations, ring-opening polymerizations, kinetic and thermodynamic studies, NMR spectra, GPC traces, DSC and TGA curves, tensile testing, and stress relaxation data.
Actions

Comments

Comments are not moderated before they are posted, but they can be removed by the site moderators if they are found to be in contravention of our Commenting Policy [opens in a new tab] - please read this policy before you post. Comments should be used for scholarly discussion of the content in question. You can find more information about how to use the commenting feature here [opens in a new tab] .
This site is protected by reCAPTCHA and the Google Privacy Policy [opens in a new tab] and Terms of Service [opens in a new tab] apply.