Identification of Durable and Non-Durable FeNx Sites in Fe-N-C Materials for Proton Exchange Membrane Fuel Cells

preprint
submitted on 12.02.2020 and posted on 13.02.2020 by Jingkun Li, Moulay-Tahar Sougrati, andrea Zitolo, James Ablett, ismail can oguz, Tzonka Mineva, ivana matanovic, plamen atanassov, andrea di cicco, Kavita Kumar, Laetitia Dubau, frédéric maillard, Frederic Jaouen
While Fe-N-C materials are a promising alternative to platinum for catalyzing oxygen reduction in acidic polymer fuel cells, limited understanding of their operando degradation restricts rational approaches towards improved durability. Here we show that Fe-N-C catalysts initially comprising two distinct FeNx sites (S1 and S2) degrade via the transformation of S1 into iron oxides while the structure and number of S2 were unmodified. Structure-activity correlations drawn from end-of-test 57Fe Mössbauer spectroscopy reveal that both sites initially contribute to the ORR activity but only S2 significantly contributes after 50 h of operation. From in situ 57Fe Mössbauer spectroscopy in inert gas coupled to calculations of the Mössbauer signature of FeNx moieties in different electronic states, we identify S1 to be a high-spin FeN4C12 moiety and S2 a low- or intermediate spin FeN4C10 moiety. These insights lay the ground for rational approaches towards Fe-N-C cathodes with improved durability in acidic fuel cells.

History

Email Address of Submitting Author

frederic.jaouen@umontpellier.fr

Institution

CNRS

Country

France

ORCID For Submitting Author

0000-0001-9836-3261

Declaration of Conflict of Interest

the authors declare no conflict of interest

Exports

Logo branding

Exports